Optical constants of PbSe (Lead selenide)
Zemel et al. 1965: n 5–10 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=\frac{21.1λ^2}{λ^2-1.37^2}$$Notes
300 K (27 °C)
References
F. Weiting and Y. Yixun.
Temperature effects on the refractive index of lead telluride and zinc selenide.
Infrared Phys. 30, 371-373, 1990
(fitting experimental data with dispersion formula: refractiveindex.info)
Data
Additional information
About Lead selenide
Lead selenide (PbSe) is a semiconducting material with noteworthy sensitivity to infrared radiation. Due to its ability to detect infrared, it finds applications in photodetectors, especially for the mid-infrared range. This makes PbSe detectors beneficial for various technologies, including thermal imaging and spectroscopy. Additionally, PbSe is researched for potential uses in photovoltaic cells and other optoelectronic devices. However, as with other lead compounds, precautions should be taken due to the potential toxicity of lead.
Other names and variations
- PbSe
- Lead(II) selenide
Links