Optical constants of PEDOT:PSS
Chen et al. 2015: n,k 0.3–1.1 µm
Wavelength:
µm
(0.3019–1.0977)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
PEDOT:PSS (Clevios AI 4083) thin film.
References
C.-W. Chen, S.-Y. Hsiao, C.-Y. Chen, H.-W. Kang, Z.-Y. Huang, H.-W. Lin. Optical properties of organometal halide perovskite thin films and general device structure design rules for perovskite single and tandem solar cells. J. Mater. Chem. A 3, 9152-9159 (2015) (Data points extracted from Supplementary materials, Figure S2)
Data
Additional information
About PEDOT:PSS
Other names and variations
- Clevios AI 4083
- Poly(3,4-ethylenedioxythiophene) polystyrene sulfonate
Links