Optical constants of PBDB-T:ITIC
Kerremans et al. 2020: n,k 0.37–1.6 µm

Wavelength: µm
 (0.3733–1.6045)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

PBDB-T:ITIC (1:1) thin film.

References

R Kerremans, C. Kaiser, W. Li, N. Zarrabi, P. Meredith, A. Armin. The optical constants of solution-processed semiconductors—new challenges with perovskites and non-fullerene acceptors. Adv. Opt. Mater. 8, 2000319 (2020) (Data points extracted from Figure 4, PBDB-T:ITIC, Ellipsometry)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About PBDB-T:ITIC

Applications: Solar cells

PBDB-T chemical composition: (C68H78O2S8)n

ITIC chemical composition: C94H82N4O2S4