RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of P3HT:PC61BM
Stelling et al. 2017: n,k 0.247–1.685 µm

Wavelength: µm
 (0.24718–1.68492)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Isotropic P3HT:PC61BM thin film (thickness 80 nm) on silicon substrate.

References

C. Stelling, C. R. Singh, M. Karg, T. A. F. König, M. Thelakkat, M. Retsch. Plasmonic nanomeshes: their ambivalent role as transparent electrodes in organic solar cells. Sci. Rep. 7, 42530 (2017) (See Supplementary information. Numerical data kindly provided by Tobias König)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About P3HT:PC61BM

Applications: Solar cells

P3HT chemical composition: (C41H53FO4S4)n

PC61BM chemical composition: C72H14O2

Links