Optical constants of Olympus IMMOIL-F30CC
Wang et al. 2017: k 1.2–1.9 µm
Wavelength:
µm
(1.200–1.900)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 295
Notes
22 °C.
References
K. Wang, W. Wen, Y. Wang, K. Wang, J. He, J. Wang, P. Zhai, Y. Yang, P. Qiu. Order-of-magnitude multiphoton signal enhancement based on characterization of absorption spectra of immersion oils at the 1700-nm window. Opt. Express 25, 5909-5916 (2017)
Data
Additional information
About Immersion oils
Oil immersion is a technique used to increase the resolving power of a microscope
Links