RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of O2 (Oxygen)
Smith et al. 1976: n 0.168–0.289 µm

Wavelength: µm
 (0.18430–0.28824)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 273.15
pressure: 101325

Notes

Standard conditions: 0 °C (273.15 K), 760 torr (101.325 kPa).

References

P. L. Smith, M. C. E. Huber, W. H. Parkinson. Refractivities of H2, He, O2, CO, and Kr for 168≤λ≤288 nm. Phys Rev. A 13, 199-203 (1976)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Oxygen

Oxygen (O2) is a diatomic molecule that constitutes about 20.8% of Earth's atmosphere. It is essential for the respiration of most life forms and is a key player in combustion processes. In its liquid and solid states, oxygen is pale blue. Optically, oxygen is generally transparent in the visible region, but it can have strong absorption bands in the ultraviolet and infrared wavelengths. This absorption is vital for protecting life on Earth by filtering out the sun's harmful ultraviolet radiation in the upper atmosphere. In advanced optical applications, oxygen plays a role in the formation of certain oxide materials used in optics, like optical fibers and waveguides. Additionally, pure oxygen environments are sometimes used in various laser processes due to its reactive nature.

Other names and variations

  • O2

Links