Optical constants of Ni (Nickel)
Werner et al. 2009: n,k 0.0176–2.48 µm

Wavelength: µm
 (0.017586–2.479684)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Experimental data: Derived from reflection electron energy-loss spectroscopy (REELS) spectra.

References

W. S. M. Werner, K. Glantschnig, C. Ambrosch-Draxl. Optical constants and inelastic electron-scattering data for 17 elemental metals. J. Phys Chem Ref. Data 38, 1013-1092 (2009)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Nickel

Nickel (Ni) is a silvery-white, lustrous metal with a slight golden tinge. It belongs to the transition metals and is hard, ductile, and ferromagnetic. In optics, nickel is commonly used as a coating material. Nickel coatings can be applied to various substrates to provide protection, reduce reflectance, or to promote adhesion for subsequent coatings. Moreover, electroplated nickel can serve as a mold surface for the precision replication of optical components. Beyond its optical applications, nickel is extensively used in many other industries, primarily in the production of stainless steel and other nickel alloys. It is also a key component in rechargeable battery systems, like those found in electric vehicles and portable electronics. Nickel's natural resistance to corrosion and its alloying properties make it a valuable metal in various engineering applications.