RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Ni (Nickel)
Rakić et al. 1998: Lorentz-Drude model; n,k 0.248–6.20 µm

Wavelength: µm
 (2.4797e-01–6.1992e+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Fit of experimental data from several sources to Lorentz-Drude (LD) model

References

A. D. Rakić, A. B. Djurišic, J. M. Elazar, M. L. Majewski. Optical properties of metallic films for vertical-cavity optoelectronic devices. Appl. Opt. 37, 5271-5283 (1998)
[Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Nickel

Nickel (Ni) is a silvery-white, lustrous metal with a slight golden tinge. It belongs to the transition metals and is hard, ductile, and ferromagnetic. In optics, nickel is commonly used as a coating material. Nickel coatings can be applied to various substrates to provide protection, reduce reflectance, or to promote adhesion for subsequent coatings. Moreover, electroplated nickel can serve as a mold surface for the precision replication of optical components. Beyond its optical applications, nickel is extensively used in many other industries, primarily in the production of stainless steel and other nickel alloys. It is also a key component in rechargeable battery systems, like those found in electric vehicles and portable electronics. Nickel's natural resistance to corrosion and its alloying properties make it a valuable metal in various engineering applications.

Other names and variations

  • Ni

Links