Optical constants of Nb-Sn (Niobium-tin alloy)
Golovashkin et al. 1971: n,k 1–10 µm; 22 wt% Sn

Wavelength: µm
 (1.0–10.0)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

22 wt% Sn; room temperature.

References

A. I. Golovashkin, E. D. Donner, I. S. Levchenko, G. P. Motulevich. Optical properties and electronic characteristics of alloys of niobium with tin, Sov. Phys. JETP 32, 1064-1067 (1971)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Niobium-tin alloy

Other names and variations

  • Nb-Sn
  • Niobium stannide
  • Triniobium-tin

Links