RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Nb:RbTiOPO4 (Niobium-doped rubidium titanyl phosphate, Nb:RTP)
Carvajal et al. 2007: n(x) 0.4–1.5 µm

Wavelength: µm
 (0.4–1.5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=2.4753+\frac{0.6664λ^{2}}{λ^2-0.0578}-0.0180λ^{2}$$

Conditions

temperature: 293
optical_component: x

Notes

Rb0.955Ti0.955Nb0.045OPO4; nx; 293 K (20 °C).

References

J. J. Carvajal, P. Segonds, A. Peña, J. Zaccaro, B. Boulanger, F. Díaz, M. Aguiló. Structural and optical properties of RbTiOPO4:Nb crystals. J. Phys. Condens. Matter. 19, 116214, 2007

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Niobium-doped rubidium titanyl phosphate

Other names and variations

  • Nb:RbTiOPO4
  • Nb:RTP