Optical constants of Nb (Niobium)
Golovashkin et al. 1969: n,k 0.40–9.2 µm; 4.2 K

Wavelength: µm
 (0.40–9.20)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 4.2

Notes

4.2 K (-268.95 °C)

References

A. I. Golovashkin, I. E. Leksina, G. P. Motulevich and A. A. Shubin. The optical properties of niobium, Sov. Phys. JETP 29, 27-34 (1969)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Niobium

Niobium (Nb) is a soft, grey, ductile transition metal, often recognized for its high melting point and unique superconducting properties. In the realm of optics, niobium's most noteworthy application lies in its thin film form, which can be utilized as a coating for specialized optical components. These coatings benefit from niobium's ability to provide excellent reflectivity in the infrared spectrum. Furthermore, due to its superconducting capabilities, niobium finds applications in advanced scientific equipment like particle accelerators and quantum computing setups, where it is used to fabricate superconducting radio-frequency (RF) cavities.