Optical constants of Nb (Niobium)
Golovashkin et al. 1969: n,k 0.40–10 µm; 293 K
Complex refractive index (n+ik)
Derived optical constants
Conditions
temperature: 293
Notes
293 K (19.85 °C)
References
A. I. Golovashkin, I. E. Leksina, G. P. Motulevich and A. A. Shubin. The optical properties of niobium, Sov. Phys. JETP 29, 27-34 (1969)
Data
Additional information
About Niobium
Niobium (Nb) is a soft, grey, ductile transition metal, often recognized for its high melting point and unique superconducting properties. In the realm of optics, niobium's most noteworthy application lies in its thin film form, which can be utilized as a coating for specialized optical components. These coatings benefit from niobium's ability to provide excellent reflectivity in the infrared spectrum. Furthermore, due to its superconducting capabilities, niobium finds applications in advanced scientific equipment like particle accelerators and quantum computing setups, where it is used to fabricate superconducting radio-frequency (RF) cavities.
Other names and variations
- Nb
Links