Optical constants of Nanoscribe IP-S
Mavrona et al. 2023: Uncured; n,k 200–998 µm
Wavelength:
µm
(199.861–997.678)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Nanoscribe IP-S photoresist for direct laser writing. Uncured.
References
E. Mavrona, A. Theodosi, K. Mackosz, E. Perivolari, I. Utke, J. Michler, J. Schwiedrzik, M. Kafesaki, O. Tsilipakos, A. Xomalis. Refractive index measurement of IP-S and IP-Dip photoresists at THz frequencies and validation via 3D photonic metamaterials made by direct laser writing. Opt. Mater. Express, 13, 3355-3364 (2023) (Numerical data kindly provided by Angelos Xomalis)
Data
Additional information
About Resists
In semiconductor fabrication, a resist is a thin layer used to transfer a circuit pattern to the semiconductor substrate which it is deposited upon. (from Wikipedia)
Links