Optical constants of NaCl (Sodium chloride)
Li 1976: n 0.20–30 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2-1=0.00055+\frac{0.19800λ^2}{λ^2-0.050^2}+\frac{0.48398λ^2}{λ^2-0.100^2}+\frac{0.38696λ^2}{λ^2-0.128^2}+\frac{0.25998λ^2}{λ^2-0.158^2}+\frac{0.08796λ^2}{λ^2-40.50^2}+\frac{3.17064λ^2}{λ^2-60.98^2}+\frac{0.30038λ^2}{λ^2-120.34^2}$$Notes
297 K (24 °C).
References
H. H. Li.
Refractive index of alkali halides and its wavelength and temperature derivatives.
J. Phys. Chem. Ref. Data 5, 329-528 (1976) and references therein.
- Sellmeier formula is derived by critical analysis of experimental data from several sources.
Data
Additional information
About Sodium chloride
Sodium chloride (NaCl), commonly known as table salt, is a white crystalline compound. In its purified form, it is transparent and can be shaped into clear optical windows. With its wide transparency range that extends from the ultraviolet through to the infrared spectrum, NaCl finds significant utility in the optics field. It's particularly well-suited for infrared spectroscopy. However, being hygroscopic, it readily absorbs moisture from the air, which can degrade its optical performance. Thus, careful handling and storage are essential when using it for optical applications.
Mineral: Halite
Other names and variations
- NaCl
- Salt
- Common salt
- Table salt
- Rock salt
- Halite
Links