Optical constants of MoSe2 (Molybdenum diselenide)
Zotev et al. 2023: n,k(o) 0.36–1.0 µm

Wavelength: µm
 (0.360–1.000)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: o

Notes

Multilayer crystals. In-plane (ordinary ray, o). Room temperature.

References

P. G. Zotev, Y. Wang, D. Andres-Penares, T. Severs-Millard, S. Randerson, X. Hu, L. Sortino, C. Louca, M. Brotons-Gisbert, T. Huq, S. Vezzoli, R. Sapienza, T. F. Krauss, B. D. Gerardot, A. I. Tartakovskii. Van der Waals materials for applications in nanophotonics. Laser and Photonics Rev. 17, 2200957 (2023) (Numerical data kindly provided by Panaiot Zotev)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Molybdenum diselenide

Molybdenum diselenide (MoSe2) is a layered compound similar in structure to molybdenum disulfide (MoS2). Each layer consists of a plane of molybdenum atoms sandwiched between two planes of selenium atoms. These layers are held together by weak van der Waals forces, allowing them to be easily exfoliated. In its bulk form, MoSe2 behaves as an indirect bandgap semiconductor. However, when reduced to a monolayer, its properties shift, and it becomes a direct bandgap semiconductor. This transition in electronic properties has attracted considerable interest in the fields of optoelectronics and nanotechnology. Potential applications include use in transistors, photodetectors, and other electronic or optoelectronic devices, especially when high-quality thin films or single layers are employed.

Other names and variations

  • MoSe2
  • Molybdenum selenide
  • Diselanylidenemolybdenum

Links