Optical constants of MoS2 (Molybdenum disulfide)
Ermolaev et al. 2020: bulk; n(o),k 0.290–3.30 µm

Wavelength: µm
 (0.290–3.300)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

optical_component: o

Notes

Ordinary optical constants (o).
In-plane component of dielectric tensor measured by spectroscopic ellipsometry.

References

G. A. Ermolaev, Yu. V. Stebunov, A. A. Vyshnevyy, D. E. Tatarkin, D. I. Yakubovsky, S. M. Novikov, D. G. Baranov, T. Shegai, A. Y. Nikitin, A. V. Arsenin, V. S. Volkov. Broadband optical properties of monolayer and bulk MoS2. NPJ 2D Mater. Appl., 4, 21 (2020) (Numerical data kindly provided by Georgy Ermolaev)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Molybdenum disulfide

Molybdenum disulfide (MoS2) is a naturally occurring, dark gray or black compound that feels similar to graphite. This similarity is due to its layered structure where each molybdenum atom is sandwiched between two sulfur atoms in a trigonal prismatic coordination. The layers are held together by weak van der Waals forces, allowing them to easily slide over each other. This property renders MoS2 useful as a lubricant in various applications. Optically, MoS2 has gained significant attention because, when exfoliated to single layers, it behaves as a direct bandgap semiconductor, making it highly relevant for optoelectronic devices. Thin layers of MoS2 have been investigated for their use in transistors, sensors, and other nanoscale devices due to their unique electronic and optical properties.