Lajaunie et al. 2013: n,k(z) 0.019–24.8 µm

Wavelength: µm
 (1.90745E-2–2.47968E+1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

direction: z

Comments

α-MoO3; nz, kz.

References

L. Lajaunie, F. Boucher, R. Dessapt, P. Moreau. Strong anisotropic influence of local-field effects on the dielectric response of α-MoO3. Phys. Rev. B 88, 115141 (2013)
(using [numerical data](https://refractiveindex.info/download/data/2013/Lajaunie 2013 - Dielectric function of alpha-MoO3.csv) made publicly available by Luc Lajaunie)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Molybdenum trioxide

Molybdenum trioxide (MoO3) is a compound of molybdenum and oxygen. It appears as an odorless, light-colored crystalline solid. It is a primary component in the production of molybdenum metal. In the field of optics, thin films of MoO3 can be deposited on various substrates, serving as layers in certain optoelectronic devices due to its semiconducting properties. The compound is also investigated for potential uses in energy storage and sensor applications. Additionally, its transparency to infrared radiation makes it a candidate for specific optical applications in the IR range.