Optical constants of Mo (Molybdenum)
Werner et al. 2009: DFT calculations; n,k 0.0176–2.48 µm
Complex refractive index (n+ik)
Derived optical constants
Notes
Theoretical density function theory (DFT) calculations.
References
W. S. M. Werner, K. Glantschnig, C. Ambrosch-Draxl. Optical constants and inelastic electron-scattering data for 17 elemental metals. J. Phys Chem Ref. Data 38, 1013-1092 (2009)
Data
Additional information
About Molybdenum
Molybdenum (Mo) is a silver-white, hard, transition metal. Known for its high melting points, strength, and resistance to corrosion, especially at high temperatures, it is invaluable in applications that demand materials capable of withstanding intense heat, such as in the production of furnace equipment and as filaments for light bulbs. In optics, molybdenum mirrors are favored for their robustness and durability, especially in high-power laser applications. The metal's reflective properties make it suitable for use as a coating for certain wavelengths, particularly in the deep ultraviolet spectral region.
Other names and variations
- Mo
Links