Optical constants of Mn (Manganese)
Johnson and Christy 1974: n,k 0.188–1.937 µm

Wavelength: µm
 (0.188–1.937)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Room temperature

References

P. B. Johnson and R. W. Christy. Optical constants of transition metals: Ti, V, Cr, Mn, Fe, Co, Ni, and Pd. Phys. Rev. B 9, 5056-5070 (1974)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Manganese

Manganese (Mn) is a transition metal with a silvery-gray appearance. It's essential in the steel industry, where it is used primarily as an alloying agent, enhancing strength, hardness, and wear resistance. In terms of optical applications, manganese can be used as a dopant in various phosphorescent and fluorescent materials, altering their luminescent properties. For instance, manganese-doped zinc sulfide is a popular phosphor, emitting a distinct orange-red light upon excitation.

Other names and variations

  • Mn

Links