Optical constants of Microchem SU-8 3000
Spec sheet: n 0.32–1.7 µm
Wavelength:
µm
(0.32–1.7)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n=1.5525+0.00629λ^{-2}+0.0004λ^{-4}$$Notes
Microchem SU-8 3000 permanent epoxy negative photoresist
References
[Microchem SU-8 3000 Data Sheet](https://refractiveindex.info/download/data/2011/Microchem SU-8 3000 Data Sheet.pdf), 2011
Data
Additional information
About Resists
In semiconductor fabrication, a resist is a thin layer used to transfer a circuit pattern to the semiconductor substrate which it is deposited upon. (from Wikipedia)
Links