Optical constants of MgO:LiNbO3 (Magnesium oxide doped lithium niobate)
Gayer et al. 2008: CLN, 5 mol % MgO; n(o) 0.5–1.7 µm

Wavelength: µm
 (0.5–1.7)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=5.6533+\frac{0.1185}{λ^2-0.2091^{2}}+\frac{89.61}{λ^2-10.85^{2}}-1.97\text{×}10^{-2}λ^{2}$$

Conditions

temperature: 297.65
optical_component: o

Notes

24.5 °C. Ordinary optical constants (o). Congruently grown lithium niobate (CLN) doped with 5 mol. % MgO. See the original publication for temperature-dependent refractive index equations.

References

O. Gayer, Z. Sacks, E. Galun, A. Arie. Temperature and wavelength dependent refractive index equations for MgO-doped congruent and stoichiometric LiNbO3. Appl. Phys. B 91, 343-348 (2008). Also see Erratum.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Magnesium oxide doped lithium niobate

Other names and variations

  • MgO:LiNbO3

Links