Optical constants of MgO (Magnesium monoxide)
Synowicki and Tiwald 2004: n,k 0.13–33 µm

Wavelength: µm
 (1.3010e-01–3.3000e+01)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Data generated from oscillator model.

References

R.A. Synowicki and T. E. Tiwald. Optical properties of bulk c-ZrO2, c-MgO and a-As2S3 determined by variable angle spectroscopic ellipsometry. Thin Solid Films 455-456, 248-255 (2004)
Calculation scripts (Python): Synowicki 2004 - MgO.py, Synowicki 2004 - Aux funcs.py

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Magnesium monoxide

Magnesium oxide (MgO) is a white solid that exhibits refractory and insulating properties. It's commonly used in the ceramics industry and for producing crucibles. In thin film form, MgO serves as an excellent substrate for the growth of high-quality epitaxial films and is transparent in the ultraviolet to infrared regions, making it suitable for various optical applications.

Mineral: Periclase

Other names and variations

  • MgO
  • Magnesia
  • Magnesium(II) oxide
  • Magnesium oxide
  • Periclase

Links