Optical constants of MgO (Magnesium monoxide)
Stephens and Malitson 1952: n 0.405–0.768 µm

Wavelength: µm
 (0.4047–0.7679)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=2.957019+\frac{0.0216485}{λ^2-0.0158650}-0.0101373λ^{2}$$

Notes

30 °C. This formula gives more accurate values for visible than the other formula describing the entire transmission range.

References

R. E. Stephens and I. H. Malitson. Index of refraction of magnesium oxide. J. Res. Natl. Bur. Stand. 49 249-252 (1952)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Magnesium monoxide

Magnesium oxide (MgO) is a white solid that exhibits refractory and insulating properties. It's commonly used in the ceramics industry and for producing crucibles. In thin film form, MgO serves as an excellent substrate for the growth of high-quality epitaxial films and is transparent in the ultraviolet to infrared regions, making it suitable for various optical applications.

Mineral: Periclase

Other names and variations

  • MgO
  • Magnesia
  • Magnesium(II) oxide
  • Magnesium oxide
  • Periclase

Links