Optical constants of MgF2 (Magnesium fluoride)
Franta et al. 2017: n,k 0.0275–125 µm
Complex refractive index (n+ik)
Derived optical constants
Conditions
film_thickness: 1.342E-7 substrate: c-Si
Notes
Film MgF2; Deposited by e-beam evaporation on c-Si; 134.2 nm thick film with an polycrystalline structure; Heterogenous data processing combining ellipsometric and spectrophotometric measurements; Room temperature.
References
D. Franta, D. Nečas, A. Giglia, P. Franta, I. Ohlídal. Universal dispersion model for characterization of optical thin films over wide spectral range: Application to magnesium fluoride. Appl. Surf. Sci. 421, 424–429 (2017) (Numerical data kindly provided by Daniel Franta)
Data
Additional information
About Magnesium fluoride
Magnesium fluoride (MgF2) is a transparent crystalline material known for its outstanding transmission properties in the ultraviolet to infrared spectrum. It is birefringent and often used in optical components such as windows, lenses, prisms, and polarizers. MgF2 is commonly applied as a protective antireflection coating on optical elements due to its high laser damage threshold, making it especially valuable for applications involving intense ultraviolet light, like those in excimer lasers. Its resistance to mechanical and thermal shocks, coupled with its transparency, also makes it suitable for use in rugged environments and outer space applications.
Other names and variations
- MgF2
- Magnesium difluoride
- Magnesium(II) fluoride
Links