RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of MgAl2O4 (Magnesium aluminate, spinel)
Chernova et al. 2017: n,k 0.14–1.67 µm

Wavelength: µm
 (1.4089e-01–1.6755e+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

MgAl2O4, magnesium aluminate spinel (MAS)

References

E. Chernova, C. Brooks, D. Chvostova, Z. Bryknar, A. Dejneka, M. Tyunina. Optical NIR-VIS-VUV constants of advanced substrates for thin-film devices. Opt. Mater. Express 7, 3844–3862 (2017)
[Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Magnesium aluminium oxide

Magnesium aluminium oxide, commonly known as spinel (MgAl2O4), is a transparent ceramic material with a cubic crystal structure. Spinel possesses excellent optical transparency from the ultraviolet to the mid-infrared range, making it valuable for various optical applications. This material is notably durable, resistant to attack from harsh environments, and can withstand high temperatures. These characteristics make it ideal for protective windows in specific high-stress applications. Moreover, due to its favorable mechanical properties and refractive index, spinel is being considered for anti-reflective coatings and other advanced optical devices. Additionally, its non-birefringent nature is a plus in certain optical scenarios.

Mineral: Spinel

Other names and variations

  • MgAl2O4
  • Magnesium aluminum oxide
  • Spinel

Links