RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Mg:LiTaO3 (Magnesium-doped lithium tantalate)
Moutzouris et al. 2011: n(e) 0.450–1.551 µm; 8 mol.% Mg

Wavelength: µm
 (0.45–1.551)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula

$$n^2=4.49361274-0.02299905λ^{2}+0.09659086λ^{-2}-1.0505035\text{×}10^{-3}λ^{-4}+6.30479079\text{×}10^{-4}λ^{-6}$$

Conditions

optical_component: e

Notes

8 mol% Mg-doped congruent lithium tantalate (MCLT). Extraordinary ray(e). 22 °C (see the original publication for temperature-dependent dispersion formula).

References

K. Moutzouris, G. Hloupis, I. Stavrakas, D. Triantis, M.-H. Chou. Temperature-dependent visible to near-infrared optical properties of 8 mol% Mg-doped lithium tantalate. Opt. Mater. Express 1, 458-465 (2011)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Magnesium-doped lithium tantalate

Other names and variations

  • Mg:LiTaO3

Links