RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of LuAl3(BO3)4 (Lutetium aluminium borate, LuAB)
Fang et al. 2013: n(e) 0.266–1.34 µm

Wavelength: µm
 (0.266–1.338)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=2.85939+\frac{0.01511}{λ^2-0.01429}-0.01116λ^{2}$$

Conditions

temperature: 298
optical_component: e

Notes

25 °C. Extraordinary optical constants (e).

References

S. Fang, H. Liu, L. Huang, N. Ye. Growth and optical properties of nonlinear LuAl3(BO3)4 crystals. Opt. Express 21, 16415-16423 (2013)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lutetium aluminium borate

Lutetium aluminium borate (LuAl3(BO3)4, or LuAB) is a synthetic crystal material known for its non-linear optical properties. With a high damage threshold and phase matching capabilities, it has potential in frequency conversion applications, especially in the deep ultraviolet to infrared spectrum. Additionally, when doped with certain rare-earth ions, LuAB can serve as a luminescent material. Its unique combination of properties makes it an attractive choice for various optical devices and systems, especially where high-power laser interactions are involved.

Other names and variations

  • LuAl3(BO3)4
  • LuAB