Optical constants of Lu3Al5O12 (Lutetium aluminium garnet, LuAG)
Hrabovský et al. 2021: n 0.193–1.69 µm
Wavelength:
µm
(0.193–1.69)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.077+\frac{1.237λ^{2}}{λ^2-0.1376^{2}}-0.0104λ^{2}$$References
J. Hrabovský, M. Kučera, L. Paloušová, L. Bi, M. Veis. Optical characterization of Y3Al5O12 and Lu3Al5O12 single crystals. Opt. Mater. Express 11, 1218-1223 (2021)
Data
Additional information
About Lutetium aluminium garnet
Lutetium aluminium garnet (Lu3Al5O12, or LuAG) is a synthetic garnet crystal. Owing to its outstanding properties, such as high density, high thermal conductivity, and good transparency in the visible and near-infrared regions, it's widely used in scintillator applications for high-energy photon detection. Additionally, LuAG has been studied as a potential host material for solid-state lasers, particularly when doped with rare-earth ions. Its transparency and luminescent characteristics make it valuable in various optical and photonic devices.