Optical constants of Lu2O3 (Lutetium sesquioxide)
Medenbach et al. 2001: n 0.435–0.644 µm

Wavelength: µm
 (0.435–0.644)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{2.609λ^2}{λ^2-0.01722}$$

References

O. Medenbach, D. Dettmar, R. D. Shannon, R. X. Fischer, W. M. Yen. Refractive index and optical dispersion of rare earth oxides using a small-prism technique. J. Opt. A: Pure Appl. Opt. 3, 174-177, 2001

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lutetium sesquioxide

Lutetium sesquioxide (Lu2O3) is a white, crystalline compound of lutetium. This material is characterized by its high melting point and stability. In the realm of optics, Lu2O3 is known for its excellent scintillation properties, making it suitable for radiation detection applications. It is often used as a scintillating crystal in detectors, and its high atomic number aids in the efficient detection of gamma rays. Moreover, its transparency in the infrared region can be harnessed in specialized optical applications.