Optical constants of Lu2O3 (Lutetium sesquioxide)
Kaminskii et al. 2008: n 0.365–2.325 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2=3.61968+\frac{0.04131}{λ^2-0.0238}-0.00856λ^{2}$$Notes
Room temperature
References
A. A. Kaminskii, M. Sh. Akchurin, P. Becker, K. Ueda, L. Bohatý, A. Shirakawa, M. Tokurakawa, K. Takaichi, H. Yagi, J. Dong. Mechanical and optical properties of Lu2O3 host-ceramics for Ln3+ lasants. Laser Phys. Lett. 5, 300-303, 2008
Data
Additional information
About Lutetium sesquioxide
Lutetium sesquioxide (Lu2O3) is a white, crystalline compound of lutetium. This material is characterized by its high melting point and stability. In the realm of optics, Lu2O3 is known for its excellent scintillation properties, making it suitable for radiation detection applications. It is often used as a scintillating crystal in detectors, and its high atomic number aids in the efficient detection of gamma rays. Moreover, its transparency in the infrared region can be harnessed in specialized optical applications.
Other names and variations
- Lu2O3
- Lutetium(III) oxide
- Dilutetium trioxide
- Lutetium oxide
Links