Optical constants of LightPath - Infrared glass (BD)
BDNL4
Wavelength:
µm
(1–15.5)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Conditions
temperature: 293
Notes
20 °C.
References
[BLACK DIAMOND BDNL4 Glass Datasheet (revision 2024-04-04)](https://refractiveindex.info/download/data/2024/BDNL Sell Sheet_4_3_2024.pdf)
Data
Additional information
Properties of BDNL4
density:
-
value: 4500
thermal_expansion:
-
value: 2.52E-5
thermal_dispersion:
-
type: dn/dT
temperature: 295
wavelength_range: 8 12
value: -1.63E-5
-
type: dn/dT
temperature: 295
wavelength_range: 3 5
value: -1.43E-5
-
type: dn/dT
temperature: 295
wavelength_range: 1 2
value: -9.7E-6
transformation_temperature:
-
value: 478
thermal_conductivity:
-
value: 0.17
hardness:
-
type: Vickers
value: 1480000000
youngs_modulus:
-
value: 14200000000