RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of LightPath - Infrared glass (BD)
BD6

Wavelength: µm
 (2–14)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 293

Notes

20 °C.

References

BLACK DIAMOND BD6 Glass Datasheet (revision 2023-07-28)
See also [datasheet revision 2018-03-02](https://refractiveindex.info/download/data/2018/LPTHCORP-1512_BD6 Glass DataSheet.pdf) for more information.

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of BD6

density:
  - 
    value: 4630
thermal_expansion:
  - 
    value: 2.25E-5
thermal_dispersion:
  - 
    type: dn/dT
    wavelength_range: 8 12
    value: 3.05E-5
transformation_temperature:
  - 
    value: 458