Optical constants of LightPath - Infrared glass (BD)
BD-2

Wavelength: µm
 (3–14)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

All values represent glass characteristics after molding

References

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

Properties of BD-2

density:
  - 
    value: 4670
hardness:
  - 
    type: Knoop
    value: 1470000000
youngs_modulus:
  - 
    value: 22100000000
thermal_expansion:
  - 
    value: 1.4E-5
thermal_dispersion:
  - 
    type: dn/dT
    value: 9.1E-5
transformation_temperature:
  - 
    value: 551