RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of LiIO3 (Lithium iodate)
Herbst 1976: n(e) 0.546–5.0 µm

Wavelength: µm
 (0.5461–5)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=0.83086+\frac{1.08807λ^2}{λ^2-0.0313810}+\frac{0.554582λ^2}{λ^2-158.76}$$

Conditions

optical_component: e

Notes

Room temperature. Extraordinary optical constants (e).

References

Cited as "R. L. Herbst (private communication)" in M. M. Choy and R. L. Byer. Accurate second-order susceptibility measurements of visible and infrared nonlinear crystals. Phys. Rev. B 14, 1693-1706 (1976).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lithium iodate

Lithium iodate (LiIO3) is a white crystalline compound that has nonlinear optical properties, making it useful in certain optical applications such as frequency conversion and electro-optical modulation. Due to its good phase-matching capabilities, it is often employed in second harmonic generation (SHG) and other nonlinear optical processes. Lithium iodate is also characterized by its relatively high damage threshold, which makes it suitable for high-power optical systems. However, the compound is sensitive to moisture and must be handled and stored under controlled conditions to maintain its optical characteristics.

Other names and variations

  • LiIO3

Links