Optical constants of LiF (Lithium fluoride)
Li 1976: n 0.10–11 µm

Wavelength: µm
 (0.1–11)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{0.92549λ^2}{λ^2-0.07376^2}+\frac{6.96747λ^2}{λ^2-32.790^2}$$

Notes

297 K (24 °C).

References

H. H. Li. Refractive index of alkali halides and its wavelength and temperature derivatives. J. Phys. Chem. Ref. Data 5, 329-528 (1976) and references therein.

  • Sellmeier formula is derived by critical analysis of experimental data from several sources.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lithium fluoride

Lithium fluoride (LiF) is a simple ionic compound commonly used in optics and radiation detection. It is transparent over a broad spectral range, from ultraviolet to mid-infrared wavelengths. This characteristic makes it an ideal material for specialized UV and IR windows and lenses. It also serves as a mount for samples to be studied by X-ray crystallography. One of its notable features is its high resistance to radiation damage, making it useful in environments with high-energy radiation. However, it is relatively soft and is moisture-sensitive, requiring careful handling to maintain its optical properties.