Optical constants of LiCl (Lithium chloride)
Li 1976: n 0.17–16 µm

Wavelength: µm
 (0.17–16)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=1.51+\frac{0.24λ^2}{λ^2-0.137^2}+\frac{9.11λ^2}{λ^2-49.26^2}$$

Notes

297 K (24 °C).

References

H. H. Li. Refractive index of alkali halides and its wavelength and temperature derivatives. J. Phys. Chem. Ref. Data 5, 329-528 (1976) and references therein.

  • Sellmeier formula is derived by critical analysis of experimental data from several sources.

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lithium chloride

Lithium chloride (LiCl) is a salt with a range of applications, from hygroscopic uses in air conditioning and industrial drying to a role as a brazing flux for aluminum in metallurgy. In the realm of optics, lithium chloride is employed as a crystal for IR, THz, and far-IR spectroscopy. It has a broad transmission range and is relatively inert, making it useful for specialized applications that require transparency in those wavelength ranges. However, it is highly hygroscopic and must be carefully handled and stored to maintain its optical properties.

Other names and variations

  • LiCl