Optical constants of LiCaAlF6 (Lithium calcium aluminum fluoride, LiCAF)
Woods et al. 1991: n(o) 0.4–1.0 µm

Wavelength: µm
 (0.4–1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2=1.92552+\frac{0.00492}{λ^2-0.00569}-0.00421λ^{2}$$

Conditions

temperature: 299
optical_component: o

Notes

26 °C. Ordinary optical constants (o).

References

B. W. Woods, S. A. Payne, J. E. Marion, R. S. Hughes, L. E. Davis. Thermomechanical and thermo-optical properties of the LiCaAlF6:Cr3+ laser material. J. Opt. Soc. Am. B 8, 970-977 (1991).

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lithium calcium aluminum fluoride

Lithium calcium aluminum fluoride (LiCaAlF6, or LiCAF) is a crystalline material with applications in solid-state lasers, especially those emitting in the ultraviolet spectrum. This material is valued for its high damage threshold and its ability to be doped with various rare-earth ions for different lasing properties. LiCAF is also known for its wide transparency range in the ultraviolet to the infrared regions, making it versatile for various optical applications. Overall, its unique combination of properties makes it a material of interest for advanced laser systems and other specialized optical uses.