Optical constants of LiCaAlF6 (Lithium calcium aluminum fluoride, LiCAF)
Woods et al. 1991: n(e) 0.4–1.0 µm
Complex refractive index (n+ik)
Derived optical constants
Dispersion formula
$$n^2=1.92155+\frac{0.00494}{λ^2-0.00617}-0.00373λ^{2}$$Conditions
temperature: 299 optical_component: e
Notes
26 °C. Extraordinary optical constants (e).
References
B. W. Woods, S. A. Payne, J. E. Marion, R. S. Hughes, L. E. Davis. Thermomechanical and thermo-optical properties of the LiCaAlF6:Cr3+ laser material. J. Opt. Soc. Am. B 8, 970-977 (1991).
Data
Additional information
About Lithium calcium aluminum fluoride
Lithium calcium aluminum fluoride (LiCaAlF6, or LiCAF) is a crystalline material with applications in solid-state lasers, especially those emitting in the ultraviolet spectrum. This material is valued for its high damage threshold and its ability to be doped with various rare-earth ions for different lasing properties. LiCAF is also known for its wide transparency range in the ultraviolet to the infrared regions, making it versatile for various optical applications. Overall, its unique combination of properties makes it a material of interest for advanced laser systems and other specialized optical uses.
Other names and variations
- LiCaAlF6
- LiCAF
Links