Optical constants of LiB3O5 (Lithium triborate, LBO)
Chen et al. 1989: n(x) 0.289–1.06 µm
Wavelength:
µm
(0.2894–1.064)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Dispersion formula
$$n^2=2.45768+\frac{0.0098877}{λ^2-0.026095}-0.013847λ^{2}$$Conditions
optical_component: x
Notes
nx; Room temperature.
References
- C Chen, Y. Wu, A. Jiang, B. Wu, G. You, R. Li, S. Lin.
New nonlinear-optical crystal: LiB3O5.
J Opt. Soc. Am. 6, 616-621 (1989)
- F. Hanson and D. Dick.
Blue parametric generation from temperature-tuned LiB3O5.
Opt. Lett. 16, 205-207 (1991).
- Ref. 2 provides a dispersion formulas based on the experimental data from Ref. 1
Data
Additional information
About Lithium triborate
Lithium triborate (LiB3O5, commonly abbreviated as LBO) is a nonlinear optical crystal that is highly useful for frequency conversion processes, including second and third harmonic generation, sum and difference frequency generation, and optical parametric oscillation. LBO crystals offer wide transparency ranges, broad phase-matching capabilities, and high damage thresholds, making them ideal for high-power laser applications. It is also appreciated for its good mechanical and thermal stability. Overall, LBO is a versatile and widely-used material in various optical and laser-based technologies.
Other names and variations
- LiB3O5
- LBO
Links