RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Li:C12H4N4 (Lithium:tetracyanoquinodimethane, Li:TCNQ )
Querry 1985: n,k 0.21–55.6 µm

Wavelength: µm
 (0.2100–55.5556)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Lithium:Tetracyanoquinodimethane (Li:TCNQ).

References

M. R. Querry. Optical constants, Contractor Report CRDC-CR-85034 (1985)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lithium:tetracyanoquinodimethane (Li:TCNQ), Li:C12H4N4