RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Li (Lithium)
Mathewson and Myers 1971: n,k 0.326–1.77 µm; 298 K

Wavelength: µm
 (0.32627–1.77120)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 298

Notes

298 K (24.85 °C)

References

A. G. Mathewson and H. P. Myers. Absolute values of the optical constants of some pure metals. Phys. Scr. 4, 291-292 (1971)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lithium

Lithium (Li) is a soft, silvery-white alkali metal that is the lightest metal and the lightest solid element. It is highly reactive and flammable, requiring special handling and storage procedures. In the context of optics and photonics, lithium is used as a component in various optical materials like lithium niobate (LiNbO3) and lithium tantalate (LiTaO3), which are commonly used for nonlinear optics, modulators, and other optical devices due to their high electro-optic coefficients. Additionally, lithium is used in the manufacturing of specialty glasses and ceramics, contributing to their desirable optical properties. Although lithium itself is not used in optical applications, its compounds are highly valuable in the field.

Other names and variations

  • Li

Links