Optical constants of LaF3 (Lanthanum fluoride)
Rodríguez-de Marcos et al. 2017: n,k 0.03–2.0 µm

Wavelength: µm
 (2.99274E-02–2.00663E+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

deposition_temperature: 523

Notes

48 nm film prepared by evaporation from tungsten boat at 250 °C

References

L. V. Rodríguez-de Marcos, J. I. Larruquert, J. A. Méndez, J. A. Aznárez. Self-consistent optical constants of MgF2, LaF3, and CeF3 films. Opt. Mater. Express 7, 989-1006 (2017) (Numerical data kindly provided by Juan Larruquert)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lanthanum fluoride

Lanthanum fluoride (LaF3) is a white, crystalline, inorganic compound that is used in a variety of optical applications. It is a popular choice for the production of fluoride glass and is also used as a scintillation material in radiation detection. Due to its low refractive index, it is often used in antireflection coatings, especially for infrared optics. The compound is stable, has good thermal durability, and exhibits a wide transparency range, making it a versatile material for various optical systems. Its low solubility in water also makes it preferable in moisture-sensitive applications. LaF3 is an important material in both research and commercial optical technologies.

Mineral: Fluocerite-(La)

Other names and variations

  • LaF3
  • Lanthanum trifluoride
  • Lanthanum(III) fluoride
  • Fluocerite-(La)

Links