Optical constants of LaAlO3 (Lanthanum aluminate)
Chernova et al. 2017: n,k 0.14–1.67 µm

Wavelength: µm
 (1.4089e-01–1.6755e+00)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Lanthanum aluminate, LaAlO3 (LAO)

References

E. Chernova, C. Brooks, D. Chvostova, Z. Bryknar, A. Dejneka, M. Tyunina. Optical NIR-VIS-VUV constants of advanced substrates for thin-film devices. Opt. Mater. Express 7, 3844–3862 (2017)
[Calculation script (Python)]

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Lanthanum aluminate

Lanthanum aluminate, LaAlO3 (LAO), has been regarded as an ideal substrate material for epitaxial growth of 1-2-3 type superconducting thin films due to a close lattice match within 1 percent as well as its low dielectric constant and loss tangent compared to other common substrate materials.