Optical constants of LZOS - Optical glass
TF3

Wavelength: µm
 (0.3650–2.3254)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

References

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About

Lytkarino Optical Glass Factory (LZOS) is a Russian company specializing in the production of high-quality optical glass and optical components. Located in Lytkarino, near Moscow, the factory has a rich history dating back to the Soviet era and has been a key player in the Russian optics industry. LZOS produces a broad range of optical materials, including various types of crown and flint glasses, which are used in telescopes, microscopes, and other high-precision optical systems. The company is known for its meticulous quality control and rigorous manufacturing standards, attributes that have garnered it both domestic and international clientele. Over the years, LZOS has expanded its capabilities to include not just the manufacturing of optical glass, but also the development and production of complex optical systems, such as lenses and mirrors for astronomical observatories. With a reputation for technical excellence, Lytkarino Optical Glass Factory is a respected name in the global optics community, providing specialized solutions for projects that demand the highest levels of optical performance and reliability.

Links