RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Kr (Krypton)
Sinnock and Smith 1969: Liquid at 126 K; n 0.363–0.644 µm

Wavelength: µm
 (0.3631–0.6439)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Conditions

temperature: 126

Notes

Liquid krypton at 126 K (-147.15 °C).

References

A. C. Sinnock and B. L. Smith. Refractive indices of the condensed inert gases. Phys. Rev. 181, 1297-1307 (1969)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Krypton

Krypton (Kr) is a noble gas with limited chemical reactivity, but it has several important applications in the field of optics. It is used as a fill gas in various types of gas lasers, including krypton-ion lasers, which produce light in the visible and ultraviolet spectra. These lasers are employed in applications ranging from scientific research to entertainment. Krypton is also used in fluorescent lamps and as a trace gas in double- or triple-pane window insulation to reduce heat transfer. It is generally safe to handle but can act as a simple asphyxiant in high concentrations.

Other names and variations

  • Kr

Links