RefractiveIndex.INFO

Refractive index database

nk database   |   n2 database   |   raw data + AI   |   about

Shelf

Book

Page

Optical constants of Kr (Krypton)
Börzsönyi et al. 2008: n 0.4–1.0 µm

Wavelength: µm
 (0.4–1)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Dispersion formula [ i ]

$$n^2-1=\frac{26102.88\text{×}10^{-8}λ^2}{λ^2-2.01\text{×}10^{-6}}+\frac{56946.82\text{×}10^{-8}λ^2}{λ^2-10.043\text{×}10^{-3}}$$

Conditions

temperature: 273
pressure: 100000

Notes

273 K (0 °C), 1000 mbar.
Dispersion formula may be usable down to ~0.2 µm.

References

A. Börzsönyi, Z. Heiner, M. P. Kalashnikov, A. P. Kovács, K. Osvay. Dispersion measurement of inert gases and gas mixtures at 800 nm. Appl. Opt. 47, 4856-4863 (2008)

Data

[Expressions for n]   [CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Krypton

Krypton (Kr) is a noble gas with limited chemical reactivity, but it has several important applications in the field of optics. It is used as a fill gas in various types of gas lasers, including krypton-ion lasers, which produce light in the visible and ultraviolet spectra. These lasers are employed in applications ranging from scientific research to entertainment. Krypton is also used in fluorescent lamps and as a trace gas in double- or triple-pane window insulation to reduce heat transfer. It is generally safe to handle but can act as a simple asphyxiant in high concentrations.

Other names and variations

  • Kr

Links