Optical constants of Kapton
Kumar et al. 2011: n 0.41–0.65 µm, k 0.49–0.78 µm

Wavelength: µm
 (0.41–0.78)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Kapton-H polyimide

References

V. Kumar, P. Goyal, R. Gupta, S. Kumar. Tailoring of optical band gap and refractive index of heat treated Kapton-H Polyimide. Adv. Appl. Sci. Res. 2 79-85 <2011)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]