Optical constants of Kapton
Kawka and Buckius 2001: n 1.44–4.97 µm, k 1.82–4.98 µm

Wavelength: µm
 (1.44–4.98)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Fourier transform infrared (FTIR) spectroscopy is used to measure the bidirectional reflectivity of polyimide films on gold substrates in the infrared. The optical constants of cured polyimide are determined in the infrared region using a Lorentz model to characterize the absorption bands.

References

P. A. Kawka and R. O. Buckius. Optical properties of polyimide films in the infrared. Int. J. Thermophys. 22, 517–534 (2001)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Kapton

Kapton is a polyimide film developed by DuPont in the late 1960s that remains stable across a wide range of temperatures.