Optical constants of Kapton
French et al. 2009: n 0.19–1.59 µm, k 0.48–2.49 µm
Wavelength:
µm
(0.19–2.49)
Complex refractive index (n+ik)
n
k
LogX
LogY
eV
Derived optical constants
Notes
Kapton HN from DuPont Electronic Technologies
References
R. H. French, J. M. Rodríguez-Parada, M. K. Yang, R. A. Derryberry, M. F. Lemon, M. J. Brown, C. R. Haeger, S. L. Samuels, E. C. Romano, R. E. Richardson. Optical properties of materials for concentrator photovoltaic systems. 2009 34th IEEE Photovoltaic Specialists Conference (PVSC), 2009, pp. 000394-000399
Data
Additional information
About Kapton
Kapton is a polyimide film developed by DuPont in the late 1960s that remains stable across a wide range of temperatures.
Links