Optical constants of Kapton
Brannon et al. 1985: k 0.19–0.39 µm

Wavelength: µm
 (0.19–0.39)  
 

Complex refractive index (n+ik)[ i ]


n   k   LogX   LogY   eV

Derived optical constants

Notes

Polyimide thin films which are chemically identical to Kapton thin films.

References

J. H. Brannon, J. R. Lankard, A. I. Baise, F. Burns, J. Kaufman. Excimer laser etching of polyimide. J. Appl. Phys. 58, 2036-2043 (1985)

Data

[CSV - comma separated]   [TXT - tab separated]   [Full database record]

Additional information

About Kapton

Kapton is a polyimide film developed by DuPont in the late 1960s that remains stable across a wide range of temperatures.

Links